Stress Rupture And Creep Testing Machine Test Metal

Stress Rupture And Creep Testing Machine Test Metal

50000.00 - 500000.00 INR/Pack

Product Details:

X

Stress Rupture And Creep Testing Machine Test Metal Price And Quantity

  • 50000.00 - 500000.00 INR/Pack
  • 1 Pack

Stress Rupture And Creep Testing Machine Test Metal Trade Information

  • 10 Pack Per Month
  • 10-30 Days

Product Description

Stress Rupture And Creep Testing Machine Test Metal, Alloy Under High Temperature

Features of Stress Rupture And Creep Testing Machine Test Metal, Alloy Under High Temperature

  • This Series creep testing machine applies advanced servo motor and ball screw actuator which assure loading conveniently and simply. The drive system comprises a printed circuit motor with toothed belt and gearbox to the recirculating ball screw actuator.
  • Motorized draw-head assembly automatically compensates for specimen elongation and keeps loading bar with excellent load accuracy of +/- 0.5% guaranteed.
  • Both room temperature and elevated temperature systems are available
  • Furnace and chambers available with temperature ranges from 200C to 1100Cin common air environments
  • Numerous high temperature pull rods, specimen holders, furnace systems and extensometers available for creep and stress Relaxation applications. Many of which are also adaptable to hot tensile testing applications on universal testing machines.
  • Control system owns the three closed control function as load control, extension control, and velocity control. High precise control and accurate load with load measurement resolution reach 1/300000; the loading testing curve can be plotted automatically.
  • Additionally, manual operation also be offered, users can unload to protect the apparatus by hand, especial the load cell, when suddenly power cut off.
  • Software owns powerful function offering specimens registration, apparatus control, test data acquisition and store, test result inquiring, data processing and test report export
  • Remote communication control function saves your operators invigilation during testing process; alarm message can be transmitted to your mobile phone to inform you test situation by equipping with special dial number device.

Technical Specifications

Model

DICTM004

Force range (kN)

0.2-50

Calibration accuracy

class 0.5/1

Force accuracy

0.5%/ 1%

Force fluctuation

0.5%/ 1%

Force resolution (minimum weight set)

1N

Axis alignment

10%

Extension measurement range(mm)

0-10mm

Extension accuracy

0.5%

Force rage (N/s)

3000

Lower pull rod travel (mm)

200

Lower pull rod speed (mm/min)

0.05-100

Leveling motor power

1000W

Dimension

7805802260(mm)

Furnace type

Three-zone, open

Temperature range

200~1100C

Uniform temperature zone

>150mm

Inside dimension

110350mm

Outside dimension

310450mm

Heating power

3kW

Temperature fluctuation

300~600C: 2C

600~900C: 3C

900~1100C: 4C

Creep Measurement

Max temperature

1000C

Measurement range

0-10mm

Accuracy

0.5%

Resolution

0.001mm

 



Tell us about your requirement
product

Price:

Quantity
Select Unit

  • 50
  • 100
  • 200
  • 250
  • 500
  • 1000+
Additional detail
Mobile number

Email

Other Products in 'Creep Testing Machine' category



trade india member
DIDAC INTERNATIONAL All Rights Reserved.(Terms of Use)
Developed and Managed by Infocom Network Private Limited.